Tunnel Oxide

A 3D NAND tunnel-oxide film stack is the innermost of the three conformal films lining a memory-hole sidewall — roughly 5 to 8 nanometers of silicon dioxide sitting directly against the channel polysilicon, thin enough that electrons can tunnel through it on command yet thick enough to hold that charge for a decade without leaking back out. Working outward from the hole's center, the deposition order runs channel poly, then tunnel oxide, then charge-trap nitride, then blocking oxide against the etched silicon-oxide/silicon-nitride (or silicon-oxide/doped-polysilicon in a gate-first OPOP stack) mold — but the films themselves are built in the opposite, outermost-first sequence, because each one has to coat the sidewall of an already-etched hole before the next, narrower film can be deposited inside it. Samsung, SK Hynix, Micron, Kioxia, SanDisk/Western Digital, and YMTC all build some variant of this ONO (oxide-nitride-oxide) sandwich — tunnel oxide, charge-trap nitride, and blocking oxide are this site's three companion film-stack articles — and the tunnel layer is the one that sets how fast a cell can be programmed and how long it can be trusted to remember what it stored.

Memory-hole etch complete
60-180+ layer ONON mold, aspect ratio often 50:1-70:1
Blocking-oxide ALD
outermost ONO film, against the mold sidewall, ~6-10 nm
Charge-trap-nitride LPCVD
Si3N4 trap layer, ~5-7 nm, the storage medium itself
Tunnel-oxide ALD / ISSG
innermost ONO film, ~5-8 nm SiO2, against the future channel
Channel-poly fill decision gatehole diameter left after three conformal films must still clear for poly deposition
Diameter check passes
undoped channel poly deposited, hole fills from sidewall inward
Diameter check fails
ONO stack too thick for remaining aspect ratio, lot scrapped or re-centered

The thickness number is a direct tradeoff, not a target chosen for its own sake. Fowler-Nordheim tunneling current rises roughly exponentially with the electric field across the oxide, and the field for a given program voltage rises as the oxide gets thinner — so a tunnel oxide at 5 nanometers programs and erases markedly faster than one at 8 nanometers, because more electrons cross per microsecond at the same applied voltage. But the same thinness that speeds tunneling during program/erase also lets trapped electrons leak back out during years of quiet storage, through the same basic tunneling mechanism running in reverse at a much lower, unintended field. Every 3D NAND tunnel-oxide recipe is a negotiation between those two failure modes: too thin and the part fails its data-retention spec (the industry benchmark is roughly 10 years at the rated operating temperature, with higher temperatures accelerating electron loss sharply); too thick and program/erase times stretch out, write latency rises, and endurance suffers because higher voltages are needed to force the same tunneling current through the extra thickness, which stresses the oxide and the trap layer behind it on every single cycle.

Memory-Hole Sidewall ONO Stack — Tunnel-Oxide Detail cross-section through one word-line layer, channel core at left Channel polysilicon (core) Word-line gate (W or Mo) Tunnel oxide Charge-trap nitride Blocking oxide electron tunneling during PROGRAM channel → trap nitride, Fowler-Nordheim, field-driven Tunnel-oxide design tension Typical thickness: 5-8 nm SiO2 Thinner → program/erase: faster Thinner → data retention: shorter Thicker → program/erase: slower Thicker → data retention: longer Retention target: 10 yr at rated temp Deposition tools: ALD / ISSG Tool vendors: Applied, Lam, TEL, ASM every recipe sits on this curve — no thickness wins on both axes at once conformal ALD or in-situ steam oxidation (ISSG) coats every one of 60-180+ layers through a single >50:1 aspect-ratio hole same tunneling path also governs the memory-channel film stack's eventual read/program electrical behavior

Depositing it is harder than the number implies. A 5-to-8-nanometer film sounds trivial next to logic's multi-hundred-nanometer interconnect dielectrics, but it has to land at that exact thickness, uniformly, on the sidewall of a hole that can run 50:1 to 70:1 or deeper in aspect ratio through 64, 96, 128, 176, or more stacked layers — a geometry where line-of-sight deposition methods simply cannot reach the bottom of the hole at all. Atomic layer deposition builds the film one self-limiting monolayer at a time through sequential precursor and oxidant pulses, which is slow but gives the conformality a >50:1 hole demands; in-situ steam generation (ISSG) is the other production route some fabs use for the tunnel layer specifically, growing the oxide thermally rather than depositing it, which can yield a denser, lower-defect-density film at the channel interface where leakage current is most sensitive to interface traps. Either way, thickness has to hold within roughly half a nanometer from the top tier to the bottom tier of the stack, because a tunnel oxide that drifts thinner at tier 150 than at tier 10 gives that tier a different effective program voltage and a different retention curve than its neighbors — a known contributor to the tier-to-tier threshold-voltage spread that 3D NAND controllers compensate for with per-tier read-voltage calibration tables.

Read the tunnel oxide through a controlled-leak lens, not a simple-insulator lens: its entire job is to leak charge in one specific, voltage-triggered direction during program and erase while refusing to leak it spontaneously for ten years of storage, and the 5-to-8-nanometer window along with the ALD/ISSG process control that holds it there across 180-plus layers is what keeps that one deliberate leak from becoming an accidental one. Everything this stack sits between — the charge-trap nitride that actually stores the bit and the blocking oxide that keeps the gate from stealing it — only works because the tunnel oxide in the middle enforces that asymmetry layer after layer, hole after hole, across an entire 3D NAND die.

Take tunnel oxide further

Ask the copilot about this term, or have our engineers assess it against your process.