GAA Dummy Gate
A GAA dummy-gate film stack is a sacrificial poly/oxide structure that wraps every suspended nanosheet in the channel column, not just a single planar surface, standing in for the real high-k metal gate through every high-temperature step that would otherwise destroy it. The dummy oxide forms a thin conformal liner across the top, bottom, and both sidewalls of each released nanosheet inside the stack, and the dummy polysilicon fills the remaining gaps between sheets and caps the structure above — a genuinely three-dimensional wrap that has no equivalent in a planar or even a FinFET dummy gate, which only ever contacts one or three faces of a solid fin. This full-wrap geometry exists because by the time the dummy gate goes down, the nanosheets are already suspended as discrete released sheets inside the channel region, each one needing its own temporary support on every exposed surface or the stack simply isn't mechanically or electrically ready for the processing that follows.
The wrap-around geometry is what forces GAA dummy-gate integration into a fundamentally different deposition sequence than any prior transistor generation. A FinFET dummy gate only has to coat three sides of a solid fin standing on the substrate, so a single conformal poly deposition over the fin topography does the job. A GAA dummy gate instead has to thread dummy oxide and dummy poly through the narrow vertical gaps between stacked nanosheets — typically 10-15 nanometers of inter-sheet spacing at the 3-nanometer-class node geometries TSMC and Samsung are now running in N2 and SF2 production — while still fully encasing each sheet's top, bottom, and both sidewalls. Lam Research's dummy-gate poly deposition tools and Applied Materials' Centura-platform CVD chambers both run specialized low-temperature recipes tuned for exactly this aspect-ratio problem, because a void or pinch-off between sheets during dummy-gate fill leaves a gap that later shows up as an uncontrolled seam in the replacement-metal-gate stack.
Outer-spacer deposition happens directly on top of the dummy-gate stack, and the two structures are built back-to-back for a reason. As this site's GAA outer-spacer film stack article covers, the SiN or SiOCN sidewall sleeve goes down on the dummy-gate flank specifically because the source/drain recess etch that comes next is aggressive enough to cut clean trenches through the stacked Si/SiGe superlattice, and the dummy-gate's polysilicon core needs that spacer standing guard so the recess chemistry doesn't eat into — and distort — the gate length the dummy structure is supposed to be preserving. Skipping straight from dummy-gate fill to S/D recess without the intervening spacer step would let the etch undercut the dummy poly at exactly the interface where gate length gets defined, so the two film stacks function as a single protective unit even though they're deposited and characterized separately.
Pattern fidelity in the dummy-gate stack propagates directly into the final transistor, which is why its removal is being tracked as a distinct, still-pending step in this GAA build sequence. The dummy oxide and dummy poly set the exact cavity geometry — length, height, and the per-sheet gap spacing — that the replacement-metal-gate stack will later have to fill without voids, so any dimensional drift introduced during dummy-gate patterning or during the high-temperature anneals it survives shows up as gate-length or threshold-voltage variation in the finished device. Pulling the dummy structure cleanly out of that same four-sided wrap geometry — the step tracked separately as GAA dummy-gate removal — is one of the least forgiving etches in the entire gate-last flow precisely because it has to clear dummy material from between sheets spaced only 10-15 nanometers apart without nicking the channel surface underneath, and the replacement-metal-gate fill that follows inherits whatever cavity shape the dummy-gate removal leaves behind.
Read the GAA dummy-gate film stack as a temporary structural scaffold, not a transistor component: everything about its geometry — full four-sided wrap, inter-sheet poly fill, spacer-protected flank — exists only to be removed later, and its real measure of success is how faithfully it preserves the cavity that TSMC's N2, Samsung's SF2, and Intel's 18A nanosheet processes will eventually fill with the gate stack that actually switches the transistor.