GAA Outer Spacer

The outer spacer is a dielectric sidewall sleeve deposited directly on the dummy-gate flank before the source/drain recess etch ever touches the stack, and its entire job is to survive that etch intact so the dummy-gate's shape — and therefore the final gate length — isn't eaten away by the same chemistry that's carving out silicon for the source/drain epitaxy. In a gate-all-around nanosheet transistor the sequence runs dummy-gate deposition, then outer-spacer deposition, then S/D recess etch, then inner-spacer formation, then S/D epitaxy, then dummy-gate pull and replacement-metal-gate fill — and the outer spacer is the only thing standing between the dummy poly/oxide placeholder and an etch step that is deliberately aggressive enough to cut clean trenches through stacked Si/SiGe superlattice.

Material choice is the whole story: outer spacers are SiN or SiOCN, almost never oxide, because the S/D recess etch has to be selective enough to remove exposed silicon and SiGe sacrificial layers fast while barely touching the spacer sitting right next to it. Plasma-enhanced ALD SiN delivers roughly 5-6 GPa film stress and a wet/dry etch selectivity against the recess chemistry that typically exceeds 20:1, which is why most 7nm-and-below FinFET and early GAA integration schemes (TSMC's N5/N3 families, Samsung's 3GAE) default to it. SiOCN variants, pushed by Applied Materials and Tokyo Electron's low-k spacer programs, trade some of that etch margin for a dielectric constant around 4.0-4.5 versus SiN's 7.0-7.5 — a meaningful swap once parasitic gate-to-S/D capacitance starts dominating AC performance at sub-3nm pitches, since every picofarad of spacer capacitance directly taxes switching speed.

Thickness sets the entire downstream budget before a single nanosheet is touched. The as-deposited outer spacer typically runs 6-8nm conformal on the dummy-gate sidewall, deposited by ALD at 300-400°C rather than CVD specifically because ALD's self-limiting surface chemistry gives thickness uniformity within about 5% across the wafer — critical because that same thickness becomes the starting offset that the recess etch, and later the inner-spacer indent, both measure from. Deposit it too thick and the effective channel-to-contact spacing balloons, costing contact resistance; too thin and the dummy-gate sidewall erodes during recess, letting the etch undercut toward the channel and distort the final gate length that replacement-metal-gate fill will lock in permanently.

The outer spacer and inner spacer are frequently confused because they sound like the same feature at different scales — they are not. The outer spacer sits outboard, on the dummy-gate's vertical sidewall, deposited in a single conformal step before any nanosheet surface is exposed by etching; its job is protecting the dummy-gate profile during S/D recess. The inner spacer forms afterward, indented laterally under each individual suspended nanosheet edge (recessing the SiGe sacrificial layer and backfilling with a low-k dielectric plug) specifically to isolate the eventual replacement metal gate from the source/drain epitaxy at every one of the 3-4 stacked channel levels — a job the outer spacer, sitting on the outside of the whole stack, structurally cannot do. One film stops an etch from reaching the gate; the other blocks a short from reaching the channel internals. Intel's RibbonFET process flow and Samsung's SF2 node both treat these as two physically and temporally separate deposition modules, not one step with two names.

Getting the outer spacer wrong shows up as a specific, traceable failure mode: gate-length walk. If the SiN or SiOCN film is non-conformal — thinner at the top of a tall dummy-gate fin than at the base, a known risk once gate aspect ratios climb past 3:1 in nanosheet stacks with 4+ channel levels — the S/D recess etch attacks the exposed upper sidewall disproportionately, and the dummy-gate (and hence the eventual metal gate it's a placeholder for) ends up narrower at the top than the bottom. KLA and Applied Materials both report that cross-wafer gate-CD variation budgets at 3nm-class nodes allow only a few angstroms of such taper before timing-closure margins erode, which is why outer-spacer ALD recipes are tuned as hard for step coverage as for etch selectivity.

Dummy-Gate Deposition
poly/oxide placeholder over nanosheet stack
Outer Spacer (this row)
6-8nm SiN/SiOCN on dummy-gate sidewall
S/D Recess Etch
cuts trenches through Si/SiGe superlattice
Inner Spacer Formation
indents under each suspended nanosheet
S/D Epitaxy + RMG Fill
dummy gate pulled, replaced with metal gate
Outer Spacer vs. Inner Spacer: Location and Timing Step A — Before Recess Etch dummy gate outer spacer nanosheet stack (unetched) outer spacer fully formed, S/D region still solid Step B — After Recess + Inner Spacer dummy gate green = inner spacer (indented, per-sheet) orange = outer spacer (unchanged, outboard) S/D recessed, nanosheets edge-indented, outer spacer intact recess + inner-spacer etch

Read the outer spacer as the etch-stop for a process step, not as part of the final transistor's electrical structure. By the time replacement-metal-gate fill happens, the dummy gate it protected has already been pulled and discarded — but the gate length and profile that the real metal gate inherits were determined entirely by how well that disposable SiN or SiOCN sleeve held its 6-8nm line through the S/D recess etch. Everything the inner spacer, S/D epitaxy, and final RMG stack build on top of assumes the outer spacer already did its one job cleanly, which is why foundries treat its ALD conformality spec with the same rigor as the gate dielectric itself, even though the film is gone before the chip ever gets tested.

Take GAA outer spacer further

Ask the copilot about this term, or have our engineers assess it against your process.