GAA Sti Liner Film Stack

A GAA STI liner film stack is the thin oxide or nitride skin grown or deposited onto the sidewalls and base of the shallow-trench-isolation moat before the trench is filled, and in a GAA process that moat has to isolate a fin that is no longer a single uniform material but a released Si/SiGe superlattice standing on, or recessed into, the substrate. The liner's job is to seal the freshly etched trench sidewall — repairing plasma-etch damage, rounding the sharp corner where the trench floor meets the base of the fin, and providing a diffusion barrier so dopants and later film stacks do not leach into the isolation dielectric — before the bulk STI fill goes down on top of it. Because the GAA fin at this stage already carries the alternating Si/SiGe layers that will later be released into individual nanosheets, the liner has to form cleanly across a sidewall that is not uniform silicon the way a FinFET trench sidewall is, which is what makes this a distinct, GAA-specific film stack rather than a simple carryover from planar or FinFET isolation.

STI trench etch
RIE through Si/SiGe superlattice fin + into substrate
Sidewall liner oxidation
thermal or ISSG oxide, 2-5nm, repairs etch damage
Nitridation / liner nitride
thin SiN cap on oxide — diffusion barrier
Corner and interface control
Base-corner rounding
removes sharp trench-floor stress riser
Superlattice sidewall seal
liner must wet both Si and SiGe sub-layers evenly
Hands off to gap fill
Liner complete
trench ready for HDP-CVD / FCVD bulk dielectric
Next: STI fill film stack
topic covered separately — void-free gap fill

The liner has to perform two jobs at once that pull in opposite directions, and GAA integration tightens the tolerance on both. The first job is etch-damage repair: the trench sidewall emerges from reactive-ion etching with a layer of broken bonds, implant knock-on damage, and residual plasma-induced defects, and a thermal or in-situ-steam-generated (ISSG) oxide of roughly 2 to 5 nanometers consumes that damaged layer and regrows a clean, low-defect-density interface. The second job is corner rounding: the trench floor meets the fin base at a geometrically sharp 90-degree corner straight out of the etch step, and that corner concentrates mechanical stress badly enough to seed dislocations or leakage paths if it is left sharp, so the liner oxidation step is tuned — longer time, slightly higher temperature, sometimes a dedicated corner-round anneal — specifically to round that one feature. At FinFET-class fin pitches this was already a tight process window; at GAA fin pitches tightened further to support denser nanosheet stacking, Applied Materials' Centura oxidation chambers and Tokyo Electron's vertical furnace platforms both run liner recipes with narrower thermal budgets, because the same high-temperature liner step that rounds the corner well can also drive unwanted Ge diffusion out of the SiGe sacrificial layers sitting just above the trench, which is a defect mode that simply does not exist on a uniform-silicon FinFET fin.

GAA STI Trench: Liner Before Fill Thin conformal liner seals sidewall + rounds base corner beneath the superlattice fin substrate Si/SiGe superlattice fin liner on sidewall rounded base corner (circled) Liner thickness ~2-5nm — thin enough to not consume trench width needed for bulk fill

The liner's thickness budget is set almost entirely by what comes next, which is why this film stack is best understood as a cross-reference pair with the GAA STI fill film stack rather than a standalone step. Every nanometer the liner consumes on the sidewall is a nanometer the subsequent bulk gap-fill dielectric does not get, and at the tight fin pitches GAA nanosheet stacking enables, that tradeoff is unforgiving — a liner grown thick enough to fully heal a rough etch and round the corner generously can leave the trench too narrow for a void-free fill, while a liner grown too thin leaves residual etch damage that shows up later as isolation leakage. Samsung's and TSMC's nanosheet process integration teams tune the liner oxidation time and temperature jointly with the fill-tool recipe for exactly this reason — the two film stacks are specified as a matched pair, not independently.

Read the GAA STI liner as an interface-conditioning step, not an isolation step in its own right: its entire purpose is to hand off a clean, corner-rounded, damage-free trench surface to the GAA STI fill film stack that actually delivers the electrical isolation, and the 2-to-5-nanometer liner recipes running on Applied Materials' and Tokyo Electron's oxidation platforms today are tuned specifically around not stealing trench width from that handoff at GAA-class fin pitch.

Take GAA STI liner film stack further

Ask the copilot about this term, or have our engineers assess it against your process.