GAA Dummy Gate Patterning
The dummy-gate patterning process is what actually sets a GAA transistor's gate length, even though the material it patterns never ends up inside the finished device. This site's GAA dummy-gate film stack article covers what the sacrificial gate is made of — commonly amorphous silicon or polysilicon capped with a hard mask, deposited over the released or soon-to-be-released nanosheet channel region. This article covers the litho and etch process that carves that material into the gate shape, because the dummy gate's critical dimension at this step is the number that every later replacement-metal-gate fill has to match exactly: whatever gate length gets patterned here is the gate length the final device has, with no opportunity to widen or narrow it after the real metal gate goes in.
Choosing amorphous silicon over polysilicon is itself a CD-control decision, not a cost one. Polysilicon's grain structure, formed during deposition and any subsequent anneal, introduces line-edge roughness at the grain boundaries that becomes visible at sub-20nm gate lengths — each grain etches at a very slightly different rate, so a nominally straight gate edge comes out with a faint saw-tooth profile under high-resolution SEM. Amorphous silicon has no grain structure to roughen the edge, which is why most 3nm-class and 2nm-class GAA dummy-gate processes, including Samsung's 3GAE and TSMC's N3-family flows, use a-Si rather than poly despite poly's lower deposition cost — the CD-uniformity and line-edge-roughness penalty from grain boundaries isn't tolerable at these pitches.
EUV single-expose patterns the gate line, but the hard mask is what survives the etch and actually defines the final edge. ASML's EUV scanners resolve the gate-line grating directly at the critical layer, but the photoresist itself is too thin and too prone to pattern collapse to survive a multi-cycle a-Si etch unmodified — so the pattern gets transferred first into an intermediate hard mask (SiN or a SiN/SiOC bilayer, cross-referencing this site's GAA hard-mask film stack article) by a short selective etch, and that hard mask, not the resist, is what guides the actual gate etch through the full a-Si thickness. This two-stage transfer exists because a-Si etch chemistries (typically Cl2/HBr-based, chosen for high Si:mask etch-rate selectivity) run long enough and aggressively enough that resist alone would erode unevenly across the wafer before the etch finished, introducing exactly the CD variation the hard mask is there to prevent.
Gate-length CD budget at this step is tighter than almost anywhere else in the GAA flow because there's no corrective step after it. Foundries hold dummy-gate CD uniformity within roughly 0.5-1nm across the wafer at 3nm-class and 2nm-class gate lengths (commonly in the 12-18nm range depending on the standard-cell target), measured inline by CD-SEM sampling across multiple die per wafer. KLA's and Applied Materials' inline metrology tools flag excursions here specifically because a dummy-gate CD error doesn't get caught until the replacement-metal-gate fill reveals a gate trench that's the wrong width — by which point the nanosheet channels have already been released and the source/drain epitaxy already grown, making the error effectively unrecoverable rather than reworkable.
Litho-etch-litho-etch (LELE) cut passes still do real work even after the main gate-line grating is exposed. A single EUV grating defines parallel gate lines across the whole array, but individual transistors need those lines cut at specific points to separate one standard cell's gate from its neighbor — a second, lower-resolution 193i exposure patterns the cut-mask openings, and a second etch removes a-Si only where the cut mask allows it, leaving isolated gate segments at the exact length the standard-cell library calls for. Samsung's and TSMC's 3nm-class flows both run this grating-plus-cut sequence rather than trying to pattern every gate-length variant directly with EUV, because re-targeting an EUV mask for every standard-cell gate length would multiply mask costs that already run into the tens of millions of dollars per layer.
Read GAA dummy-gate patterning as the process that spends its entire budget on a material that gets stripped out and thrown away — because the dummy gate's only real job is to hold open, at exactly the right width, the space where the actual device will eventually live.