Psg Process
The PSG process deposits phosphosilicate glass — SiO2 doped with phosphorus alone, no boron — and it's chosen specifically for what it leaves out, not what it adds. BPSG's boron content is exactly what lowers its reflow temperature enough to planarize, but boron is also a mobile dopant that can diffuse out of the glass and into nearby silicon; PSG trades away BPSG's easy reflow specifically to avoid introducing that extra boron source anywhere near a junction that can't tolerate it.
Boron penetration from a doped glass cap is the same basic failure mode the silicon oxynitride process covers for boron diffusing out of a PMOS gate electrode, just relocated to a different source. Any sufficiently mobile boron sitting close to a thermal budget hot enough to drive diffusion can migrate into nearby silicon and shift a threshold voltage or degrade a junction's intended profile — it doesn't matter whether that boron started in a doped polysilicon gate or in a doped glass film sitting right above a sensitive structure. BPSG's boron content, so useful for lowering its own reflow temperature, becomes a liability the moment that film sits directly over a gate stack or shallow junction that genuinely can't tolerate an extra boron source nearby during a later high-temperature step.
That boron-free safety comes at the direct cost of reflow performance, because phosphorus alone doesn't disrupt the glass network nearly as much as boron and phosphorus together. PSG requires a meaningfully higher temperature than BPSG to reach the same viscous-flow planarization, if it's reflowed at all — many PSG applications are used specifically as a non-reflowed capping or passivation film rather than as a planarizing pre-metal dielectric, accepting a less-flat surface in exchange for never introducing boron near the structure it's protecting. Where BPSG is the right choice specifically because a surface needs planarizing and there's no boron-sensitive structure directly underneath, PSG is the right choice specifically when the opposite is true: gettering is still wanted, planarization either isn't needed or is handled by CMP instead, and boron absolutely cannot be allowed nearby.
Phosphorus's gettering of mobile sodium works identically in PSG as it does in BPSG, since that mechanism never depended on boron being present at all. The sodium-trapping benefit covered in the BPSG process is purely a phosphorus effect; removing boron from the film doesn't weaken that gettering in any way, which is exactly why PSG can serve as a full substitute for BPSG's ion-contamination protection in any flow that doesn't also need BPSG's lower reflow temperature.
Read the PSG process as the direct complement to BPSG: the same phosphorus chemistry doing the same sodium-gettering job, deliberately stripped of the one ingredient — boron — that would otherwise make the film dangerous to deposit directly over a boron-sensitive gate or junction, accepted in exchange for a glass that's a good deal harder to reflow into a flat surface.