Tantalum Process
The tantalum process deposits Ta and TaN as the copper damascene barrier covered in the copper process — but "the barrier" undersells what's actually there. It's almost always two distinct tantalum-based layers doing two distinct jobs, not one film doing double duty, and the reason tantalum specifically (rather than titanium, the barrier metal of choice everywhere else in the fab) got the copper assignment comes down to a property titanium doesn't share.
TaN and Ta face opposite directions in the stack, and each one is optimized for the specific material sitting on its own side, not for the barrier job in the abstract. TaN, deposited first against the dielectric trench wall, is dense and chemically stable enough to block copper diffusion into the surrounding low-k or oxide — the core barrier function — and bonds well to that dielectric surface. Pure tantalum metal, deposited on top of the TaN, faces the copper side of the stack instead, where it offers lower electrical resistance than TaN alone and — just as importantly — a surface copper wets and nucleates on cleanly, giving the PVD copper seed layer (and the electroplated fill that follows it) a reliable starting surface rather than a patchy, poorly adhered one.
Titanium does the equivalent barrier-adhesion job everywhere else in the fab, so tantalum's selection specifically for copper is itself the notable fact, not an arbitrary materials choice. The titanium process and titanium nitride process cover Ti/TiN doing adhesion and barrier duty under aluminum, under tungsten contacts, and in HKMG work-function stacks — a far broader footprint than tantalum's. Tantalum's narrower, copper-specific role exists because TaN's diffusion-blocking performance against copper specifically outperforms TiN's at the thinness barriers have to run at in advanced BEOL, and because titanium's own strong oxygen-getter chemistry (the property that makes it so useful everywhere else) turns out to interact less favorably with copper's interface chemistry than tantalum's more inert behavior does. The industry didn't standardize on tantalum for copper because titanium failed outright — it standardized on tantalum because it measurably won that one specific matchup.
Tantalum pentoxide (Ta2O5) is an entirely separate application, using the same base element in an oxide rather than a metal or nitride form, for a dielectric job unrelated to interconnect barriers. Ta2O5's relatively high dielectric constant made it a candidate high-k capacitor dielectric in DRAM storage capacitors during the era before the industry moved toward other high-k materials for that role, the same dielectric-constant-driven reasoning that pushed gate dielectrics from SiO2 to SiON to today's hafnium-based high-k stacks. That use shares tantalum's name and little else with the barrier bilayer — different compound, different electrical function, different place in the chip entirely.
Read the tantalum process as a case where the barrier job that looks, from a distance, like "one film blocking diffusion" turns out on inspection to be two films, each engineered against a different neighbor: TaN sealed to the dielectric it's protecting, Ta wetted to the copper it has to support electrically and mechanically — and tantalum earned that specific assignment by being measurably better suited to copper's particular chemistry than the titanium-based barrier that handles nearly everything else in the fab.