Titanium Nitride Process

The titanium nitride process deposits TiN — titanium's nitride, chosen everywhere titanium itself proves too reactive to leave exposed. TiN is harder, far more chemically inert, and still conductive enough to carry current through a barrier rather than block it entirely, which is the combination of properties that makes it the default cap for nearly every Ti layer in the fab and a genuinely separate deposition process in its own right, not just "titanium with extra nitrogen."

PVD route
Reactive sputter Ti target in N2/Ar
CVD/ALD route
TiCl4 + NH3, conformal
Pick by geometry and purity needline-of-sight vs. conformal coverage
PVD TiN
Dense, clean, poor via sidewall coverage
ALD TiN
Excellent conformality, Cl residue risk
NH3/H2 post-treatment
Removes residual chlorine from CVD/ALD film
Barrier or ARC cap
Conductive, stable, ready for next layer

PVD and CVD/ALD TiN aren't interchangeable, because the deposition mechanism itself decides whether the film can reach the sidewalls of a deep, narrow feature. Reactive PVD sputters titanium from a target through a plasma while flowing nitrogen gas, which reacts in flight and on the wafer surface to form TiN — a line-of-sight process that deposits well on flat, open surfaces but struggles to coat the sidewalls and bottoms of tall, narrow contacts and vias the way a true vapor-phase surface reaction can. CVD and especially ALD TiN, grown from titanium tetrachloride (TiCl4) reacting with ammonia (NH3), proceeds as a surface-limited chemical reaction that coats every exposed face at nearly the same rate regardless of geometry — the same conformality advantage TEOS has over silane-based oxide, applied here to a conductive barrier instead of a dielectric.

PVD TiN vs. ALD TiN in a High-Aspect-Ratio Via line-of-sight sputtering can't reach where a surface reaction can PVD TiN (reactive sputter) thick at the field sidewall barely coated — barrier integrity at risk ALD TiN (TiCl4 + NH3) uniform thickness, field to sidewall to bottom as contacts and vias got taller and narrower, barrier conformality — not deposition rate — became the deciding factor between PVD and ALD

That conformality advantage comes with a real cost: TiCl4-based TiN tends to trap chlorine in the as-deposited film, and leftover chlorine is a genuine reliability hazard, not a cosmetic impurity. Residual chlorine reacts with atmospheric moisture to form corrosive byproducts, and in a tungsten contact flow specifically, chlorine contamination in the TiN barrier can interact with the WF6 fluorine chemistry covered in the tungsten process in ways that degrade barrier performance exactly where it's needed most. Production ALD TiN recipes manage this with a post-deposition NH3 or H2 plasma treatment — sometimes performed between individual ALD cycles rather than only at the end — specifically to strip residual chlorine out of the growing film before it becomes trapped and immobile.

The decision between PVD and ALD TiN is, in practice, the same fill-factor argument the tungsten and cobalt processes make about barrier thickness versus conductor volume — applied to the barrier material's conformality instead of its thickness. A thinner, more uniform ALD barrier leaves more of a shrinking contact's cross-section available for the actual low-resistance fill metal, the same logic that favored cobalt's thinner liner over tungsten's thicker one; TiN's choice between deposition methods is really a choice about how evenly that limited barrier budget gets spent across a feature's geometry, not just how much of it there is.

TiN's second major job — as an anti-reflective coating cap on aluminum lines, covered in the aluminum process — relies on an entirely different property: its optical absorption at lithography wavelengths, not its barrier performance at all. The same material, deposited the same basic way, does two unrelated jobs depending on where it sits in the stack: underneath, blocking diffusion and promoting adhesion; on top of a reflective aluminum line, suppressing the standing-wave reflections that would otherwise distort the photoresist pattern above it.

Read the titanium nitride process as the natural partner to the titanium process's oxygen-getter story: titanium does the interface-cleaning work precisely because it's reactive, and TiN exists specifically to cap that reactive titanium with something stable enough to survive everything downstream — barrier duty, ARC duty, or both — while the choice between how that TiN gets deposited, PVD or ALD, comes down entirely to whether the feature underneath still has line-of-sight access or needs a surface reaction to reach it at all.

Take titanium nitride process further

Ask the copilot about this term, or have our engineers assess it against your process.