Titanium Process

The titanium process deposits Ti — almost always a thin PVD or CVD film, a few nanometers to a few tens of nanometers thick — in more structurally different roles across a modern chip than almost any other metal: an adhesion layer under barriers, a silicide-forming contact layer, a work-function metal in HKMG gate stacks, an ARC-adhesion promoter. Those roles look unrelated until they're traced back to one shared chemical property: titanium has an unusually strong affinity for oxygen, strong enough to pull oxygen out of whatever thin native oxide sits in its way, and that single getter behavior is what makes titanium useful in nearly every place it shows up.

Surface has native oxide
Any exposed Si, metal, or barrier
Ti deposited on top
PVD sputter, thin film
Titanium's oxygen affinity does the worksame mechanism, different downstream result
Getters the native oxide
Ti + O reaction, TiOx forms at Ti's own surface
Leaves a clean interface
Lower contact resistance underneath
Silicide / barrier adhesion
Reliable bonding to what's above
Work-function tuning
TiAl/TiAlC role in HKMG gate stack

Every surface exposed to air for even a moment carries a thin native oxide, and that oxide is exactly what blocks the clean, low-resistance interface most process steps actually need. Silicon forms native SiO2 within seconds of air exposure; aluminum forms native Al2O3 just as fast, as covered in the aluminum process; even many metal barrier surfaces pick up some surface oxidation between process steps. Whatever film or reaction is supposed to happen next — a silicide formation, a barrier bond, a low-resistance contact landing — has to either break through that oxide or avoid it, and titanium's specific chemistry does the former better than almost any other practical thin-film metal: titanium reacts with the oxide preferentially, pulling oxygen atoms out of the surface it's sitting on and converting them into a thin titanium oxide at its own surface instead, leaving a cleaner interface behind.

Titanium's Getter Action: One Mechanism, Three Jobs Ti pulls the native oxide's oxygen to its own surface, leaving a clean interface below Contact silicide Si (native SiO2) Ti film Ti getters the oxide, reacts with Si → silicide Barrier adhesion dielectric surface Ti film TiN barrier Ti bonds the barrier down Work-function metal HfO2 gate dielectric TiAl / TiAlC Al diffusion lowers the work function The shared mechanism underneath all three Ti's bond to oxygen is stronger than Si-O, Al-O, or most other surface oxides it contacts so Ti pulls that oxygen to itself, forming a thin TiOx skin and leaving a reduced, bondable interface underneath one chemical property, three structurally unrelated downstream uses this is also why a Ti deposition is often the very first metal layer, regardless of what gets built on top of it

That same getter action is what drives titanium silicide (TiSi2) formation, even though cobalt silicide displaced it from the narrowest contact lines for the resistance reasons the cobalt process covers. Depositing Ti directly on exposed silicon and annealing lets titanium both scavenge the native oxide and then react with the clean silicon surface underneath to form TiSi2 — the getter step and the silicide-forming reaction are two stages of essentially the same chemistry, which is why Ti silicidation doesn't need a separate oxide-removal step beforehand the way some other contact processes do.

The TiAl/TiAlC work-function metal layer covered in the gate-last HKMG stack relies on the same oxygen-scavenging property, applied to the gate dielectric instead of to silicon or a barrier surface. Depositing a titanium-aluminum alloy directly against the high-k gate dielectric lets titanium's getter behavior clean and stabilize that interface the same way it does elsewhere, while the aluminum content in the same film does the separate electrical job of lowering the stack's effective work function for NMOS. Titanium is doing its usual interface-cleaning job in that stack; the work-function tuning is aluminum's contribution riding along in the same film.

Pure titanium metal is almost never left as the final exposed surface anywhere in the stack, because the same reactivity that makes it such a good getter also makes it chemically unstable on its own. A thin Ti layer gets capped with TiN in nearly every application — the barrier role covered in the aluminum BEOL stack — specifically because TiN is far more chemically inert and mechanically robust than pure Ti, while Ti underneath keeps doing the interface-cleaning and adhesion job TiN alone wouldn't do as well directly against an oxide or silicon surface.

Read the titanium process as proof that a single, simple chemical property — an unusually strong bond to oxygen — can underwrite a half-dozen structurally different roles across a chip, as long as the surrounding system always needs the same basic favor: scavenge whatever thin oxide is in the way, and leave a cleaner, more bondable interface behind. Every place titanium shows up in this glossary — barrier adhesion, silicide formation, HKMG work-function stacks — is really the same chemistry, applied to a different surface each time.

Take titanium process further

Ask the copilot about this term, or have our engineers assess it against your process.