3D NAND Opop Mold Film Stack
A 3D NAND OPOP mold film stack is the gate-first alternative to the ONON stack this site's 3D NAND film stack article covers: instead of depositing sacrificial silicon nitride and swapping it for metal later through a slit trench, the word-line material — doped polysilicon — is deposited directly into the stack as oxide/poly/oxide/poly (OPOP) pairs, so the conductive gate is already in place the moment deposition finishes. Toshiba and SanDisk's original BiCS (Bit Cost Scalable) architecture used this scheme because it skips the replacement-gate module entirely — no hot-phosphoric-acid nitride pull-back, no multi-megawatt metal etch-back through a 100:1 aspect-ratio slit, no risk of a word line shorting to its neighbor mid-swap. The tradeoff is electrical: polysilicon word lines run at roughly 500 to 1,000 microohm-cm resistivity even after heavy doping, versus 5 to 20 microohm-cm for the tungsten or molybdenum gates that a replacement-gate (ONON) flow installs, so OPOP stacks accept higher word-line RC delay and settle for shorter decks and lower layer counts than today's 200-plus-layer gate-last designs reach.
The OPOP route still needs its own channel-hole etch, tunnel-oxide and charge-trap-nitride deposition, and channel-polysilicon fill — everything downstream of the mold stack is shared with the ONON flow this site's 3D NAND film stack and replacement-gate etch articles describe — but it never runs a slit-based metal swap, because there is nothing sacrificial left to swap. That single structural choice is why OPOP all but disappeared from leading-edge roadmaps once layer counts pushed past roughly 96 to 128 tiers: polysilicon's resistivity scales a device's word-line RC delay badly enough at that length that Samsung, SK Hynix, Micron, and Kioxia all converged on gate-last ONON-plus-metal-replacement for every generation beyond the first few BiCS-style parts. Read OPOP as the simpler, lower-risk mold stack that traded electrical performance for process simplicity, and ONON as the harder, metal-swapping stack that traded a slit-full of replacement-gate risk for the low-resistance word lines modern layer counts actually require.