3D NAND Tunnel Oxide Deposition

A 3D NAND tunnel-oxide deposition process is the atomic layer deposition or in-situ steam generation (ISSG) step that grows the 5-to-8-nanometer silicon-dioxide film against the channel core — the production chemistry and reactor mechanics that have to hit that exact thickness uniformly at the bottom of a hole that can be 50 to 70-plus diameters deep. This site's tunnel-oxide film-stack article covers why that thickness window exists — the program/erase-speed-versus-retention tradeoff the number itself represents — but the number only means anything if the deposition process can actually deliver it at every one of 64 to 176-plus tiers in a single hole, and that is a materially harder engineering problem than the thickness target alone suggests. Samsung, SK Hynix, Micron, Kioxia, SanDisk/Western Digital, and YMTC each run their own qualified recipe for this step, built around either sequential self-limiting ALD cycles or thermally grown ISSG oxide, and Applied Materials, Lam Research, Tokyo Electron, and ASM International all supply the reactor platforms fabs use to run it. What follows is the process-mechanics view of tunnel-oxide deposition specifically — precursor and oxidant chemistry, deposition temperature, and why thickness uniformity with depth, not any single-point thickness measurement, is the real metric a tunnel-oxide recipe is judged on.

Charge-trap nitride deposited
LPCVD Si3N4 already in place over the blocking oxide
Tunnel-oxide ALD cyclerepeated self-limiting half-reactions, hundreds of cycles
Precursor pulse
e.g. tris(dimethylamino)silane or similar Si precursor adsorbs as a monolayer
Purge
inert gas clears unreacted precursor before oxidant enters
Oxidant pulse
O3 or O2 plasma converts the adsorbed monolayer to SiO2
Purge + repeat
cycle repeats until target thickness is reached, self-limiting per cycle
ISSG alternative route
thermal oxidation in H2/O2 ambient, ~800-1000C, denser interface
Thickness-uniformity metrology
spectroscopic ellipsometry or TEM sampled top/mid/bottom tier

ALD and ISSG solve the same aspect-ratio problem through opposite mechanisms. Atomic layer deposition builds the tunnel oxide through alternating precursor and oxidant pulses separated by purge steps, with each half-reaction self-limiting at one monolayer regardless of how deep into the hole the gas has to travel — the chemistry caps the growth rate per cycle, which is exactly the property that makes ALD conformal through a greater-than-50:1 aspect ratio where simple flux-limited deposition would starve the bottom of the hole. In-situ steam generation instead grows the oxide thermally, reacting hydrogen and oxygen directly at the silicon surface at roughly 800 to 1000 degrees Celsius to form a denser, lower-defect-density interface than a deposited film typically achieves, which matters disproportionately for the tunnel oxide because interface-trap density at the channel boundary directly sets leakage current during the ten-year retention window. Fabs choose between the two, or combine them, based on which failure mode dominates their yield data: ALD wins when depth-uniformity is the binding constraint, ISSG wins when interface quality is.

Tunnel-Oxide Thickness Uniformity vs Hole Depth ALD vs line-of-sight deposition, sampled top to bottom of a 176-tier hole 8nm 5nm 0nm hole depth: top tier (1) → bottom tier (176) film thickness ALD, self-limiting cycles 6.1 nm top, 5.8 nm bottom — flat flux-limited deposition (not used in production) starves below ~tier 60, thickness collapses near the bottom Process Target film: 5-8 nm SiO2 ALD uniformity: within ~0.5 nm top-bottom ISSG temp: 800-1000 C ALD chemistry: Si precursor + O3/O2 plasma Aspect ratio: 50-70:1+ Metrology: ellipsometry, TEM sample Vendors: Applied, Lam, TEL, ASM a tunnel oxide that drifts thinner near the bottom tiers gives those cells a different program voltage and retention curve than tier 1 self-limiting ALD chemistry, not reactor pressure or flow alone, is what keeps the film flat across 176 tiers

Temperature and cycle count are the two levers that actually get tuned, not the precursor chemistry itself. Once a fab qualifies a precursor/oxidant pair for its reactor platform, day-to-day process control mostly comes down to deposition temperature — generally kept in a narrow band because too low slows the self-limiting surface reaction and risks incomplete monolayer formation, while too high can trigger gas-phase reactions that stop being self-limiting and reintroduce the same depth-dependent non-uniformity ALD exists to avoid — and total cycle count, which sets the final thickness directly since each cycle adds a fixed, calibrated increment. The purge step between precursor and oxidant pulses is the quieter lever: too short a purge lets residual precursor react with the incoming oxidant in the gas phase rather than on the surface, producing particles and a less controlled film; this is why mature tunnel-oxide ALD recipes spend as much qualification effort tuning purge duration as they do tuning the pulse chemistry itself, even though purge steps add no material to the film at all.

Read tunnel-oxide deposition through a depth-uniformity lens, not a single-thickness-number lens: the 5-to-8-nanometer target this site's tunnel-oxide film-stack article describes is only a meaningful spec if the same self-limiting ALD chemistry, or the same thermally grown ISSG interface, delivers it within roughly half a nanometer from tier 1 to tier 176 — and the purge-tuned, temperature-controlled cycle mechanics covered here are what actually stand between that target and a die full of cells with 176 different effective tunnel-oxide thicknesses.

Take 3D NAND tunnel oxide deposition further

Ask the copilot about this term, or have our engineers assess it against your process.