Apf Process

The APF process deposits Advanced Patterning Film — Applied Materials' trade name for a CVD amorphous carbon hard mask — as a sacrificial layer that stands between a thin photoresist pattern and the much deeper etch that pattern needs to survive. It exists to solve a problem lithography created on its own: as resist films got thinner to resolve finer features, they stopped being thick enough to survive the etches those features required.

Target layer
Oxide, poly, or metal to be etched
APF deposition
PECVD amorphous carbon, 1500–4000Å
Pattern transfer chainthin resist pattern, thick carbon does the etch work
Cap layer (DARC/SiON)
Anti-reflective, etch-selective
Thin resist litho
Fine CD, shallow depth of focus ok
Etch cap + APF
Pattern transfers into carbon
Deep target etch
APF survives as the hard mask
O2 ash strip
Carbon removes cleanly, no residue

The problem APF solves is a mismatch between what litho needs and what etch needs. Resolving ever-finer critical dimensions pushed resist films thinner and thinner, because a thick resist diffracts and defocuses the exposure light enough to blur fine patterns — but a thin resist simply doesn't have enough material to survive etching all the way through a thick target film underneath it. Amorphous carbon breaks that trade-off apart: the thin resist only has to pattern a thin cap layer, which then patterns the much thicker carbon film, which is what actually survives the long, deep etch into oxide, polysilicon, or a hard mask stack below. Each layer in the chain only has to be exactly as thick as its own step requires.

APF: Decoupling Thin Litho From Deep Etch a thin resist pattern transfers through thin layers until it reaches the thick carbon that does the real work ① The film stack Target layer (oxide / poly) APF — amorphous carbon thick, 1500–4000 Å cap layer (DARC/SiON) thin resist — fine CD only ② After pattern transfers through APF APF deep etch into target resist + cap already consumed — only carbon survived to protect this O2 plasma ash strips amorphous carbon completely afterward — no metal residue, no selective-etch legacy to manage

Carbon's real advantage is selectivity, not strength. Amorphous carbon etches very slowly relative to oxide, nitride, and polysilicon under the fluorine- and chlorine-based chemistries used to pattern those layers, which is exactly what a hard mask needs — it has to survive an etch step that's actively trying to consume everything in its path. Carbon pairs that selectivity with a property almost no other hard mask material offers: it strips away completely in an oxygen plasma ash, leaving no metal or nitride residue behind that would otherwise need its own dedicated removal step. Tungsten or titanium-nitride hard masks can deliver similar etch resistance, but getting rid of them afterward is its own process; APF's removal step is a simple ash.

APF became load-bearing for multiple patterning, not just single critical layers. Because it can be deposited thick without the optical penalties a thick resist would carry, amorphous carbon is also the material of choice as the mandrel or spacer-core film in self-aligned double and quadruple patterning schemes — the same spacer process that splits a lithography tool's native pitch in half or in quarter depends on a sacrificial core material that etches cleanly, strips completely, and doesn't contaminate the trenches it leaves behind. That combination of properties is why amorphous carbon hard masks, under APF or equivalent trade names from other equipment makers, show up throughout advanced-node front-end and back-end-of-line litho modules rather than in just one step.

Stripping APF is its own monitored step, because "ash it all off" still has an endpoint the process can't afford to miss. The carbon has to be gone completely before the next deposition, but the ash chemistry is also attacking whatever's now exposed underneath it:

APF Strip: What's Exposed Once the Carbon Burns Off the ash has to clear every trace of carbon without attacking the freshly etched target underneath Before ash APF — amorphous carbon residual mask, post deep etch freshly etched target substrate below O2 plasma — burns carbon to CO/CO2, pumped away lingering O2 exposure here can oxidize or roughen the target layer just cleared unlike a metal or nitride hard mask, carbon leaves no residue to rinse — but the ash itself still needs a stop signal

That stop signal comes from watching carbon's own combustion byproducts disappear, the same closed-loop logic every endpoint-driven etch or strip step relies on:

APF Ash Endpoint Loop carbon combustion byproducts fall to a floor the instant the film is gone O2 plasma ash burns exposed carbon Monitor CO* / CO2* combustion emission intensity Carbon exhausted? signal drops to baseline Stop short O.E. CO/CO2 signal still elevated — carbon remains, keep ashing Why a short over-etch, not a long one O2 plasma has essentially no selectivity to many target materials once carbon is gone a few extra seconds clears residual carbon in trench corners; a long over-ash just oxidizes exposed film the loop confirms carbon is fully consumed, then gets off the wafer before oxygen does anything else

And isolated from the loop diagram, this is the trace a strip module actually follows — carbon's combustion signature collapsing as the film runs out:

APF Ash Endpoint Trace CO/CO2 emission intensity vs. ash time ash time (s) CO* / CO2* intensity carbon exhausted — stop signal steady combustion while carbon remains baseline floor — brief over-ash, then off no selectivity trick here — the whole strategy is minimizing time spent in this chamber after the signal drops

Read the APF process as the fix for a trade-off lithography couldn't solve on its own: resist thickness and pattern resolution pull in opposite directions, so rather than ask resist to do a job it physically can't, the industry inserted a disposable carbon layer whose entire purpose is to be thick exactly where the etch needs it and gone completely once the etch is done — and even that disappearance is instrumented, not assumed.