GAA Contact Liner

A GAA contact-liner film stack is the thin Ti/TiN barrier that goes down between source/drain epitaxy and contact-metal fill inside a trench whose aspect ratio is tighter than anything a planar or FinFET contact process ever had to handle. The liner's job hasn't changed from earlier nodes — form a low-resistance, reliable interface to the epitaxial source/drain while blocking metal-fill species from diffusing into and contaminating the semiconductor — but the trench it has to coat has gotten narrower and deeper at the same time nanosheet source/drain epi volume shrank, which squeezes the process margin available for getting that coating right into a noticeably tighter band than FinFET or planar contact modules ever worked within.

S/D epitaxy complete
raised epi fills recess between sheets
Contact trench etched
narrow, high-aspect-ratio opening to epi
Liner deposition
Ti layer first
reacts with epi, forms low-R silicide
TiN barrier over Ti
blocks W/Ru/Co diffusion into epi
Thermal activation
RTA forms silicide interface
TiSi2/NiSi-class contact resistance reduction
Metal fill follows
Liner continuity checked first
voids here undermine entire fill

Aspect ratio is the whole reason this liner gets its own film-stack discussion instead of inheriting a FinFET recipe unchanged. A FinFET source/drain contact trench sits on top of a raised fin with a comparatively open approach angle, giving physical vapor deposition and ALD liner chemistries a reasonably forgiving line-of-sight path to the bottom of the trench. A GAA contact trench, by contrast, has to reach down through a taller stack while staying narrow enough not to bridge into the neighboring gate or an adjacent device at the tight pitches 3-nanometer-class nanosheet nodes run at — Samsung's 3GAE and TSMC's N2 both push contact pitch tighter even as the trench gets taller relative to its width, and that combination is exactly what defines a high-aspect-ratio deposition problem. Ti/TiN liners deposited by PVD lose step coverage fast as aspect ratio climbs, which is why ALD-based TiN liner chemistry — offered by Applied Materials' Endura platform and by Tokyo Electron's ALD liner modules — has become the practical default for GAA contact integration even though PVD liners remained acceptable through much of the FinFET generation.

Contact-Liner Coverage: Aspect Ratio Gets Tighter Ti/TiN liner must coat trench walls fully before metal fill — harder as the trench narrows and deepens FinFET contact trench S/D epi wide opening, open line-of-sight to bottom GAA contact trench S/D epi narrower + taller — tighter liner process margin Amber: Ti/TiN liner · cyan: S/D epitaxy. A thin or incomplete liner at the trench bottom means a direct metal-fill/epi interface the barrier was supposed to prevent — and less process margin to catch it.

The liner's chemistry does two jobs at once, and both get harder under tighter geometric constraint. The titanium layer reacts with the exposed source/drain epitaxy during a rapid thermal anneal to form a low-resistance silicide interface, directly lowering contact resistance in a way that plain metal-on-semiconductor contact never achieves on its own — the same silicidation chemistry that's made Ti- and Ni-based silicides a standard contact-resistance lever since well before FinFET. The titanium nitride layer on top of that silicide then has to fully enclose the trench sidewalls to block whatever metal-fill species comes next — tungsten, ruthenium, or cobalt — from diffusing into the epi and degrading the junction, and a thin spot or pinhole anywhere in that TiN barrier undermines the entire contact's reliability regardless of how good the fill metal itself turns out to be.

This liner and the wrap-around contact geometry it sits inside are related but distinct problems, and conflating them is a common mistake. As this site's wrap-around-contact article covers, extending a contact to reach additional source/drain faces — top and sidewalls, or in some documented embodiments the underside as well — is fundamentally a geometry decision about which semiconductor surfaces get contacted at all. The liner discussed here is the material that has to successfully coat whichever faces that geometry decision selects, so a wrap-around contact with poor liner step coverage on its sidewall faces gains none of the access-resistance benefit the extra geometry was supposed to deliver — the two have to succeed together, but neither one substitutes for the other.

Liner integrity gets verified before the metal fill step is trusted, because a liner failure caught after fill is far more expensive to fix. Cross-sectional inspection checks for void-free, continuous Ti/TiN coverage along the full trench depth, and electrical test structures separate contact resistance into its silicide, liner, and bulk-metal contributions so a problem traced back to the liner isn't misattributed to the fill metal instead. Getting that sequencing right matters more at GAA's tighter aspect ratios than it did at FinFET geometries, simply because there's less physical margin in the trench to absorb a marginal liner and still end up with an acceptable contact.

Read the GAA contact-liner film stack as the step that makes the contact trench trustworthy before anything gets filled into it: the silicide interface sets contact resistance, the TiN barrier protects the junction underneath it, and both have to hold up inside a trench aspect ratio tighter than FinFET or planar contacts ever demanded — which is exactly why GAA contact-liner integration earns its own process discipline rather than inheriting a prior-node recipe wholesale.

Take GAA contact liner further

Ask the copilot about this term, or have our engineers assess it against your process.