GAA Work-Function-Metal Film Stack

Metal gate work-function tuning solves a problem HKMG deposition order alone cannot: an NMOS transistor and a PMOS transistor sitting side by side on the same die need their threshold voltages set by two different effective work functions pulled from the same high-k dielectric and the same bulk tungsten fill, so the fab inserts thin, masked, sub-nanometer metal and dipole layers into each transistor type's gate stack before the common fill step to shift each one toward its own target. Intel's 45 nm gate-last HKMG node and every finFET and gate-all-around generation since has depended on getting this split right, because a work-function mismatch of even 50-100 mV shows up directly as a shifted threshold voltage, a leaky off-state, or a device that is slower or less efficient than its neighbor on the same wafer.

Why the same high-k stack needs two different answers

A MOSFET's threshold voltage depends on the effective work function at the gate-dielectric interface relative to the silicon band structure underneath. For an NMOS device, the fab wants the gate's effective work function pulled down near the silicon conduction band edge (roughly 4.0-4.2 eV); for a PMOS device, it wants the effective work function pulled up near the valence band edge (roughly 5.0-5.2 eV). Since both device types share the same HfO2-based high-k dielectric and the same tungsten or cobalt bulk gate fill for cost and process-integration reasons, the only place left to create that 0.8-1.0 eV split is a few angstroms of interfacial material inserted between the high-k layer and the bulk fill metal, deposited and masked separately for each transistor type.

The two tuning mechanisms fabs actually use

Metal-stack tuning stacks specific metals in a specific order: a thin titanium nitride (TiN) layer is nearly universal as a barrier and base work-function setter, and NMOS regions get an additional thin aluminum-containing capping layer (TiAlC or TiAlN, pioneered in Intel's and Samsung's gate-last flows) that pulls the effective work function down, while PMOS regions are masked off from that aluminum layer and instead keep a TiN-dominant or added tungsten-nitride stack that stays near the higher work-function target. Layer thickness in this scheme is the dial: GLOBALFOUNDRIES and TSMC HKMG process disclosures describe NMOS work-function metal thicknesses in the 1-3 nm range, where a 0.2 nm change in TiAlC thickness can shift Vt by tens of millivolts.

Dipole/cap-layer tuning, used increasingly below 14 nm and in gate-all-around nodes where the metal gate trench is too narrow for thick multi-metal stacks, instead diffuses a sub-monolayer of a lanthanide or aluminum oxide (La2O3 for NMOS, Al2O3 for PMOS) directly at the high-k/interfacial-layer boundary during a controlled anneal. The dipole forms an intrinsic electric field across that interface that shifts the effective work function without needing extra physical metal thickness in the already-crowded gate trench — critical once gate pitch scaling left less than 2 nm of lateral room per side in finFET and nanosheet transistors.

Process flow: two masks, two depositions, one fill

HKMG GATE-LAST WORK-FUNCTION TUNING SEQUENCE
  |
  1. High-k dielectric (HfO2-based) deposited conformally, ALD, across all gate trenches (NMOS + PMOS)
  |
  2. TiN barrier/base WFM layer deposited across all trenches (common to both device types)
  |
  3. Block mask #1: PMOS regions covered with photoresist/hardmask
  |      -> NMOS trenches exposed: TiAlC (or La2O3 dipole anneal) deposited, work function pulled toward
  |         conduction band (~4.0-4.2 eV target)
  |      -> strip mask #1
  |
  4. Block mask #2: NMOS regions covered with photoresist/hardmask
  |      -> PMOS trenches exposed: additional TiN/WN or Al2O3 dipole step, work function held/pulled
  |         toward valence band (~5.0-5.2 eV target)
  |      -> strip mask #2
  |
  5. In-line Vt-tuning metrology (spectroscopic ellipsometry + electrical test structures) confirms
  |  split met before committing to bulk fill
  |
  6. Bulk gate fill (tungsten, sometimes cobalt) deposited into both NMOS and PMOS trenches -> common to
     the tungsten-plug-contact-fill-process downstream
  |
  7. CMP planarizes gate fill flush with ILD -> gate stack complete, ready for contact module

Diagram 1 — NMOS vs. PMOS gate stack cross-sections and the resulting Vt split

Metal Gate Work-Function Stacks: NMOS vs. PMOS Silicon channel HfO2 high-k dielectric TiN base WFM layer TiAlC (NMOS Vt-down layer) W bulk fill NMOS gate stack Si channel HfO2 high-k TiN base layer TiAlC cap (Al pulls WF down) W bulk gate fill Effective WF ~4.1 eV Vt target: low, near conduction band PMOS gate stack Si channel HfO2 high-k TiN / WN (thicker, no Al cap) W bulk gate fill Effective WF ~5.1 eV Vt target: low-magnitude, near valence band Silicon band edges and gate work-function targets Ec ~4.05 eV NMOS WF ~4.1 eV PMOS WF ~5.1 eV Ev ~5.17 eV

Diagram 2 — Vt shift vs. tuning-layer thickness and the dipole alternative at scaled pitch

Work-Function Tuning: Thickness Dial vs. Dipole Diffusion Panel A: TiAlC thickness vs. NMOS Vt shift TiAlC thickness (nm) Vt shift (mV) 0.5nm 1.5nm 3.0nm Saturates near 3nm: trench fill margin runs out first Panel B: Dipole layer at scaled gate pitch HfO2 high-k La2O3 dipole (sub-ML) TiN W fill (no room for thick stack) Trench width <10nm: dipole shifts WF via interface field, not added metal volume

Mechanism comparison

AttributeMetal-stack tuning (TiAlC/TiN)Dipole tuning (La2O3/Al2O3)
Typical node introduced45-32 nm gate-last HKMG14 nm and below, finFET/GAA
Lateral space required1-3 nm per added layerSub-monolayer, minimal space
Primary knobLayer thicknessAnneal temperature/time, dose
Fails whenTrench too narrow for stack (advanced nodes)Diffusion uncontrolled, dipole migrates
Typical Vt shift achieved100-300 mV50-150 mV
Representative usersIntel 45nm/32nm, early GLOBALFOUNDRIES HKMGTSMC/Samsung finFET and GAA nodes

Why both NMOS and PMOS tuning steps must be verified before fill

Because the bulk tungsten (or cobalt) fill step that follows is common to both transistor types and essentially irreversible without a full gate-stack strip and rework, fabs run in-line spectroscopic ellipsometry and dedicated electrical test-structure Vt measurements after the two masked work-function depositions and before committing to fill. A miss on either side — TiAlC too thin on NMOS, or the PMOS block mask leaving residual aluminum behind that drags its work function down — shows up only after full gate stack completion as a Vt bin split or outright functional failure, by which point the fix requires scrapping the lot rather than adjusting a single layer.

Metal gate work-function tuning is the step that turns the single shared gate stack built by the high-k-metal-gate-hkmg-process into two electrically distinct transistor types on the same wafer, and it hands off a planarized, Vt-correct gate directly into the same tungsten bulk-fill and CMP sequence used downstream in the tungsten-plug-contact-fill-process — the dipole and metal-stack choices made here are what let a single gate-last integration flow serve both NMOS and PMOS without a second lithography-defined dielectric module.