GAA Fin Patterning

GAA fin patterning is the one lithography step where the etch has to cut through two different materials at once and leave both behaving like they're the same thing. Every prior fin-forming process on the roadmap, including FinFET fin patterning, only ever etched one material — bulk silicon, or a single epitaxial layer. The GAA nanosheet process starts from a grown superlattice of alternating silicon and silicon-germanium (typically 5-6 pairs at the 3nm-class node, each layer 5-8nm thick), and patterning that stack into a fin-like mesa means slicing through Si and SiGe layers simultaneously while holding the same critical dimension across both materials despite their different etch rates, different thermal budgets during the prior epitaxy step, and different strain states from the SiGe's larger lattice constant. A CD mismatch of even 1-2nm between what the Si layers see and what the SiGe layers see propagates directly into nanosheet width variation after channel release, which is why this step carries tighter CD-uniformity budgets than any single-material fin etch ever needed.

Pitch-splitting does the heavy lifting before the etch ever starts. At 3nm-class fin pitches (around 40-48nm), a single 193nm-immersion or even EUV exposure can't resolve the pattern directly, so foundries fall back to self-aligned double patterning (SADP) or self-aligned quadruple patterning (SAQP) — depositing a sacrificial mandrel, growing a conformal spacer film around it by ALD, removing the mandrel, and using the remaining spacer loops as the actual etch mask. SAQP repeats the spacer-on-spacer trick twice to quarter the pitch, which is what most 3nm and 2nm GAA flows use to reach sub-25nm half-pitch without needing a second EUV exposure. Samsung's 3GAE process and TSMC's N3/N2 both lean on SAQP-class multi-color patterning for the fin-cut layer; Intel's 18A, running full EUV single-expose for several critical layers, still uses a cut-mask step afterward to carve individual fin segments out of a continuous spacer-defined line. ASML's EUV scanners resolve the line/space grating itself at roughly 28nm pitch in a single exposure, but the fin-segment cut mask is a separate, lower-resolution step layered on top — mixing an EUV grating with a 193i cut pattern is now routine because it's cheaper than an all-EUV multi-pass flow.

The hard mask has to survive two very different etch chemistries without eroding unevenly. Patterning through a Si/SiGe superlattice means switching etch gas chemistry mid-step — commonly a fluorocarbon-based plasma (CF4/CHF3 mixes) tuned for silicon, alternated with a chlorine-based chemistry (Cl2/HBr) that attacks SiGe more aggressively because of its weaker Ge-Ge bond energy relative to Si-Si. A hard mask (typically SiN or a SiN/SiO2 bilayer, detailed in this site's GAA hard-mask film stack article) has to resist both chemistries for the full multi-cycle etch without thinning so much that line-edge roughness creeps into the final fin sidewall. Applied Materials' Centris Sym3 etch platform and Lam Research's Kiyo series both run cyclic "ALE" (atomic layer etch) sequences here — alternating a self-limiting adsorption step with a short ion-bombardment removal step — specifically because a continuous plasma etch would blow through the thin SiGe layers faster than it clears the thicker Si layers, undercutting them into a stepped, non-vertical sidewall.

Superlattice grown
5-6 Si/SiGe pairs, epi
Hard mask deposit
SiN/SiO2 bilayer
Mandrel + spacer (SAQP)
pitch quartered by ALD spacer
Mandrel removal
spacer loops remain
Cut-mask litho
segments individual fins
Cyclic ALE etch
alternating Cl2/HBr + CF4/CHF3
Fin-like mesa formed
Si/SiGe sidewall near-vertical
Mask strip + clean
feeds STI formation

Sidewall verticality is the metric that actually separates a good fin-patterning run from a bad one. Because the two materials etch at different rates under identical plasma conditions, an uncorrected process produces a scalloped sidewall — Si layers recessed less than SiGe layers, leaving a visible stair-step profile under cross-section TEM. Foundries track this as sidewall angle, targeting 88-90 degrees from horizontal across the full stack height (typically 50-70nm for a 5-6 pair superlattice plus hard mask), with less than 1nm of layer-to-layer CD difference tolerated. KLA's cross-section metrology and inline scatterometry tools are used specifically to catch scalloping before it reaches the STI fill step, because a scalloped sidewall at this stage telegraphs directly into non-uniform SiGe recess depth during the later nanosheet release etch — a defect that's far more expensive to catch after the gate stack is already formed.

Fin Sidewall: Uncontrolled vs. ALE-Corrected Etch Single continuous plasma etch Cyclic ALE (alternating chemistry) scalloped sidewall, ~2-4nm CD step near-vertical, <1nm CD difference Si layer SiGe layer Sidewall angle target: 88-90 deg | CD-uniformity budget: <1nm layer-to-layer

Read GAA fin patterning not as "the FinFET fin etch, but smaller," but as the first process step where the fab has to treat two chemically different materials as one mechanical object — a discipline that didn't exist until the superlattice-based nanosheet architecture made it mandatory, and that now sets the CD-uniformity floor every downstream GAA step, from STI formation to nanosheet release, has to live within.

Take GAA fin patterning further

Ask the copilot about this term, or have our engineers assess it against your process.